Heat Capacity of Nickel–Phosphorus Eutectic Melts
- Авторы: Kamaeva L.V.1, Lad’yanov V.I.1
-
Учреждения:
- Udmurt Federal Research Center, Ural Branch, Russian Academy of Sciences
- Выпуск: Том 57, № 2 (2019)
- Страницы: 177-181
- Раздел: Thermophysical Properties of Materials
- URL: https://journals.rcsi.science/0018-151X/article/view/157934
- DOI: https://doi.org/10.1134/S0018151X19020068
- ID: 157934
Цитировать
Аннотация
Ni–P alloys containing phosphorus from 15 to 23 at %, which is close to the eutectic concentration, are studied with differential scanning calorimetry. The heat capacity CP is calculated at a constant pressure for the melts from the obtained data. The CP values of the alloys at temperatures above their melting points at 50°C are 0.53–0.59 J/(g K) and are in good agreement with the literature heat capacity values for liquid nickel and Ni3P. The CP of all of the melts linearly increases from the ТL liquidus temperature to 1400°С. There is a maximum on the concentration dependence of CP at the eutectic concentration.
Об авторах
L. Kamaeva
Udmurt Federal Research Center, Ural Branch, Russian Academy of Sciences
Автор, ответственный за переписку.
Email: lara_kam@mail.ru
Россия, Izhevsk
V. Lad’yanov
Udmurt Federal Research Center, Ural Branch, Russian Academy of Sciences
Email: lara_kam@mail.ru
Россия, Izhevsk
Дополнительные файлы