Effect of the Density of Iron Nanopowders on the Parameters of Their Ignition during Heating in Air


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

The ignition of iron nanopowders of bulk density and those compacted to a relative density of 0.3–0.5 during heating in air has been studied. The ignition temperature of the compacted samples is independent of the heating rate and is 100–115°C. The durations of the active stages—ignition and filtration combustion—under identical heating mode depend on the sample density, which makes it possible to develop methods to store iron nanopowders in the compacted state.

Авторлар туралы

M. Alymov

Institute of Structural Macrokinetics and Problems
of Materials Science, Russian Academy of Sciences

Хат алмасуға жауапты Автор.
Email: alymov@ism.ac.ru
Ресей, Chernogolovka, Moscow oblast, 142432

S. Vadchenko

Institute of Structural Macrokinetics and Problems
of Materials Science, Russian Academy of Sciences

Email: alymov@ism.ac.ru
Ресей, Chernogolovka, Moscow oblast, 142432

E. Suvorova

Institute of Structural Macrokinetics and Problems
of Materials Science, Russian Academy of Sciences

Email: alymov@ism.ac.ru
Ресей, Chernogolovka, Moscow oblast, 142432

V. Zelenskii

Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences

Email: alymov@ism.ac.ru
Ресей, Moscow, 119991

A. Ankudinov

Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences

Email: alymov@ism.ac.ru
Ресей, Moscow, 119991

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Pleiades Publishing, Inc., 2019