Creation of a microrelief by thermally stimulated shrinkage of metal-coated polypropylene films


Cite item

Full Text

Open Access Open Access
Restricted Access Access granted
Restricted Access Subscription Access

Abstract

A study was made of the conditions of producing micron-sized reliefs by thermally stimulated shrinkage of metallized commercial biaxially oriented polypropylene films. It was shown that, in annealing within a temperature range close to the polypropylene melting point, the film shrinks in two directions to form folded structures on the surface. The folds are about 2–8 μm in size. The shrinkage and the relief depth depend on the annealing temperature. The relief remains on the film surface after the removal of the aluminum layer.

About the authors

A. Yu. Yarysheva

Moscow State University

Author for correspondence.
Email: alyonusha@gmail.com
Russian Federation, Moscow, 119992

A. A. Tunyan

Moscow State University

Email: alyonusha@gmail.com
Russian Federation, Moscow, 119992

A. V. Bol’shakova

Moscow State University

Email: alyonusha@gmail.com
Russian Federation, Moscow, 119992

D. R. Strel’tsov

Moscow State University

Email: alyonusha@gmail.com
Russian Federation, Moscow, 119992

S. N. Malakhov

National Research Center “Kurchatov Institute,”

Email: alyonusha@gmail.com
Russian Federation, Moscow, 123098

L. M. Yarysheva

Moscow State University

Email: alyonusha@gmail.com
Russian Federation, Moscow, 119992

S. N. Chvalun

National Research Center “Kurchatov Institute,”

Email: alyonusha@gmail.com
Russian Federation, Moscow, 123098

A. L. Volynskii

Moscow State University

Email: alyonusha@gmail.com
Russian Federation, Moscow, 119992

Supplementary files

Supplementary Files
Action
1. JATS XML

Copyright (c) 2017 Pleiades Publishing, Ltd.