Studying the change in characteristics of optical surfaces of a spacecraft


Cite item

Full Text

Open Access Open Access
Restricted Access Access granted
Restricted Access Subscription Access

Abstract

The change in the working characteristics of the optical element sample depending on the thickness of the contamination film applied to the sample has been estimated experimentally. As sources of contamination, the coatings of lens hoods were chosen, which are located in close proximity to the contamination- sensitive optical system of a spacecraft. A series of experiments for applying contamination films of different thickness to the sample of the optical element has been carried out. Based on preliminary estimations, the thickness of the contamination during the entire period of the active existence of the spacecraft will not exceed 3500 Å.

About the authors

A. G. Volkov

OAO Korporatsiya Kometa (Kometa Special Space Systems Corporation)

Email: natalya.d.2011@inbox.ru
Russian Federation, Moscow, 115280

N. A. Dyugaeva

OAO Korporatsiya Kometa (Kometa Special Space Systems Corporation)

Author for correspondence.
Email: natalya.d.2011@inbox.ru
Russian Federation, Moscow, 115280

G. N. Kuvyrkin

Bauman Moscow State Technical University

Email: natalya.d.2011@inbox.ru
Russian Federation, Moscow, 105005

A. N. Morozov

Bauman Moscow State Technical University

Email: natalya.d.2011@inbox.ru
Russian Federation, Moscow, 105005

Supplementary files

Supplementary Files
Action
1. JATS XML

Copyright (c) 2017 Pleiades Publishing, Ltd.