Sintering of alumina ceramic with 95% Al2O3 [VK 95-1] content with additives of aluminum oxide nanopowder and without it is studied. The increase in strength by 32 ± 3% is ensured by additives of 1.5 ± 0.5 wt %. The strength reaches 170 ± 5 MPa, which allows it to be used as dental prosthesis forms in stomatology.

作者简介

V. Vereshchagin

National Research Tomsk Polytechnic University

编辑信件的主要联系方式.
Email: oldenstom@list.ru
俄罗斯联邦, Tomsk

O. Proskurdina

Krasnoyarsk Diabetes Oral Rehabilitation Scientific Center for Patients with Diabetes

Email: oldenstom@list.ru
俄罗斯联邦, Krasnoyarsk

T. Khabas

National Research Tomsk Polytechnic University

Email: oldenstom@list.ru
俄罗斯联邦, Tomsk

S. Starosvetskiy

Krasnoyarsk Diabetes Oral Rehabilitation Scientific Center for Patients with Diabetes

Email: oldenstom@list.ru
俄罗斯联邦, Krasnoyarsk

D. Proskurdin

Krasnoyarsk Diabetes Oral Rehabilitation Scientific Center for Patients with Diabetes

Email: oldenstom@list.ru
俄罗斯联邦, Krasnoyarsk

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2016