The possibility is shown of creating a chart of local corrosion damage in the walls of heat-exchange tubes on the basis of the data of matrix eddy current testing with registration of the position, type, and depth of all local corrosion damage areas. The results of examination of condensers operated under different conditions and at different plants are used to calculate the theoretical depth distribution of defects. It is shown that, in all cases, a satisfactory statistical description of the corrosion defect depth on the cooling water size is obtained by employing the Weibull distribution. Pearson’s coefficient is in the range of 0.994–0.997.

作者简介

V. Golovin

Frumkin Institute of Physical Chemistry and Electrochemistry, Russian Academy of Sciences

编辑信件的主要联系方式.
Email: golovin@rocor.ru
俄罗斯联邦, Moscow, 119071

N. Pechnikov

NPO ROKOR LLC

Email: golovin@rocor.ru
俄罗斯联邦, Moscow, 129110

V. Shchelkov

Frumkin Institute of Physical Chemistry and Electrochemistry, Russian Academy of Sciences

Email: golovin@rocor.ru
俄罗斯联邦, Moscow, 119071

A. Tsivadze

Frumkin Institute of Physical Chemistry and Electrochemistry, Russian Academy of Sciences

Email: golovin@rocor.ru
俄罗斯联邦, Moscow, 119071

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2018