Stability of catalysts for the oxidative chlorination of methane
- Авторы: Rozanov V.N.1, Treger Y.A.1, Silina I.S.1,2
-
Учреждения:
- OOO NIITs Sintez
- Moscow State University of Fine Chemical Technologies
- Выпуск: Том 8, № 4 (2016)
- Страницы: 336-340
- Раздел: Engineering Problems. Operation and Production
- URL: https://journals.rcsi.science/2070-0504/article/view/202369
- DOI: https://doi.org/10.1134/S2070050416040085
- ID: 202369
Цитировать
Аннотация
The effects on the stability of catalysts for the oxidative chlorination of methane due to evaporation of the active component (copper chloride) of the catalyst are studied. The volatility of copper chloride is shown to depend mainly on the catalyst composition and temperature. At a moderate 350°C in the reactor, the evaporation of copper chlorides after 5 h is 0.45% on a catalyst containing copper and potassium chloride and 0.72% on a catalyst containing lanthanum chloride. The stability of catalyst operation can be effectively maintained not only by decreasing the volatility of copper chloride, but also by feeding hydrochloric acid with dissolved copper chloride isolated from the reaction gas of methane oxychlorination at the outlet of the reactor (for the removal of reaction heat and the recycling of unconverted hydrogen chloride) back into the reactor.
Ключевые слова
Об авторах
V. Rozanov
OOO NIITs Sintez
Автор, ответственный за переписку.
Email: RozanovVN@yandex.ru
Россия, Moscow, 119311
Yu. Treger
OOO NIITs Sintez
Email: RozanovVN@yandex.ru
Россия, Moscow, 119311
I. Silina
OOO NIITs Sintez; Moscow State University of Fine Chemical Technologies
Email: RozanovVN@yandex.ru
Россия, Moscow, 119311; Moscow, 119571
Дополнительные файлы