Physicomechanical properties of nickel coating deposited from sulfate nickel plating electrolyte using preliminary underpotential deposition


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

A study of nickel coatings electroplated from electrolytes of the compositions (M) NiSO4 0.5, NiCl2 0.3, and H3BO3 0.404 (electrolyte 1) and NiSO4 0.5, NiCl2 0.3, and H3BO3 0.404 with the addition of 2 mg L–1 RADO (electrolyte 2) in the constant-current mode after preliminary potentiostatic treatment (underpotential deposition) of the support revealed the formation of Fe–Ni alloy in the initial moment of formation of the nickel coating. Pretreatment of the steel surface in the underpotential deposition mode allows preparation of uniform finely crystalline nickel coatings with enhanced levels of the wear resistance, microhardness, and corrosion resistance.

Авторлар туралы

D. Legkaya

Engels Institute of Technology

Email: tepeti@mail.ru
Ресей, pl. Svobody 17, Engels, Saratov oblast, 413100

N. Solov’eva

Engels Institute of Technology

Хат алмасуға жауапты Автор.
Email: tepeti@mail.ru
Ресей, pl. Svobody 17, Engels, Saratov oblast, 413100

A. Yakovlev

Engels Institute of Technology

Email: tepeti@mail.ru
Ресей, pl. Svobody 17, Engels, Saratov oblast, 413100