Preparation of nanosized zinc oxide by vacuum oxidation and kinetic study of oxidation


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

Nanosized zinc oxide was prepared with a vacuum oxidation method by using hot-dip galvanizing slag as the raw material and air as the oxygen source. The oxidation kinetics curves of zinc vapor at different pressures were plotted by thermogravimetry, and the morphology of ZnO was observed by scanning electron microscopy. The nanosized ZnO products were hexagonal wurtzite crystals with the purity ≥99.98. When parabolic kinetics occurred, the ZnO products were granular, amorphous, tetra-needle-like or single needle-like. In the case of linear kinetics, the products were short tetra-needle-like or needle-like crystals. Zinc oxidation was controlled by the contracting spherical model R3 initially and the three-dimensional diffusion model D4 thereafter, with the apparent activation energies of 101.3–122.1 kJ/mol and 111.2–143.4 kJ/mol respectively.

作者简介

Ai Shi

School of Metallurgical and Materials Engineering

Email: zhangrljx19201@163.com
中国, Jiangsu, Zhangjiagang, 215600

Rong Zhang

School of Metallurgical and Materials Engineering

编辑信件的主要联系方式.
Email: zhangrljx19201@163.com
中国, Jiangsu, Zhangjiagang, 215600

Li Ji

School of Metallurgical and Materials Engineering

Email: zhangrljx19201@163.com
中国, Jiangsu, Zhangjiagang, 215600

Yang Zhang

School of Metallurgical and Materials Engineering

Email: zhangrljx19201@163.com
中国, Jiangsu, Zhangjiagang, 215600

Ai Huang

School of Metallurgical and Materials Engineering

Email: zhangrljx19201@163.com
中国, Jiangsu, Zhangjiagang, 215600

补充文件

附件文件
动作
1. JATS XML

版权所有 © Allerton Press, Inc., 2017