Production of CeO2 Nanoparticles by Method of Laser Ablation of Bulk Metallic Cerium Targets in Liquid


Цитировать

Полный текст

Открытый доступ Открытый доступ
Доступ закрыт Доступ предоставлен
Доступ закрыт Только для подписчиков

Аннотация

The method of pulsed laser ablation in liquid was used to synthesize dispersions of cerium oxide nanoparticles when subjecting a metallic cerium target in water and alcohol to basic frequency radiation of the nanosecond Nd:YAG laser (1064 nm, 7 ns, 20 Hz). Researchers have studied the effect of laser radiation parameters, duration of impact, and optical scheme of experiment on the ablation process. The average rate of nanoparticle production was 50 mg/h in water and 25 mg/h in alcohol. Researchers have studied the size characteristics and crystalline structure of the nanoparticles produced. The particles have bimodal size distribution with 6 nm and 25 nm maximums. The average crystallite size is 17–19 nm. The crystalline structure of nanoparticles, namely cubic cerium oxide (fluorite structure), space group Fm-3m, is confirmed by the X-ray diffraction data, as well as optical absorption spectra and Raman spectroscopy.

Об авторах

V. Svetlichnyi

V. D. Kuznetsov Siberian Physical-Technical Institute at Tomsk State University

Автор, ответственный за переписку.
Email: v_svetlichnyi@bk.ru
Россия, Tomsk

I. Lapin

V. D. Kuznetsov Siberian Physical-Technical Institute at Tomsk State University

Email: v_svetlichnyi@bk.ru
Россия, Tomsk

Дополнительные файлы

Доп. файлы
Действие
1. JATS XML

© Springer Science+Business Media New York, 2016

Согласие на обработку персональных данных

 

Используя сайт https://journals.rcsi.science, я (далее – «Пользователь» или «Субъект персональных данных») даю согласие на обработку персональных данных на этом сайте (текст Согласия) и на обработку персональных данных с помощью сервиса «Яндекс.Метрика» (текст Согласия).