Single crystals of L-histidine phosphite (L-Hist · H3РО3) have been grown from aqueous solution by slow cooling method. The results of elemental analysis, of X-ray-diffraction studies of the crystal structure, and the habitus of the obtained crystals are given. The elastic and piezoelectric coefficients have been measured on the plates with the (010) natural faces by the method of electromechanical resonance for stretching vibrations in the temperature range 295–340 K. Elastic compliance values s33 and s22 and the corresponding elastic-moduli values, piezoelectric coefficients d23 and d22, coefficients of electromechanical coupling, and temperature coefficient of the resonance frequency are obtained. A comparison is given with other crystals, which are compounds of amino acids with phosphorous or phosphoric acid.

Об авторах

E. Balashova

Ioffe Physical Technical Institute

Автор, ответственный за переписку.
Email: balashova@mail.ioffe.ru
Россия, St. Petersburg

B. Krichevtsov

Ioffe Physical Technical Institute

Email: balashova@mail.ioffe.ru
Россия, St. Petersburg

S. Popov

Ioffe Physical Technical Institute

Email: balashova@mail.ioffe.ru
Россия, St. Petersburg

P. Brunkov

Ioffe Physical Technical Institute

Email: balashova@mail.ioffe.ru
Россия, St. Petersburg

G. Pankova

Institute of Macromolecular Compounds

Email: balashova@mail.ioffe.ru
Россия, St. Petersburg

A. Zolotarev

St. Petersburg State University

Email: balashova@mail.ioffe.ru
Россия, St. Petersburg


© Pleiades Publishing, Ltd., 2018

Данный сайт использует cookie-файлы

Продолжая использовать наш сайт, вы даете согласие на обработку файлов cookie, которые обеспечивают правильную работу сайта.

О куки-файлах