Electrical Conductivity of Cancrinite-Type Na8 − 2xCax[Al6Si6O24][CO3] · 2H2O (x ≤ 0.03) Crystals
- Autores: Sorokin N.I.1
-
Afiliações:
- Shubnikov Institute of Crystallography, Federal Scientific Research Centre “Crystallography and Photonics,”
- Edição: Volume 63, Nº 3 (2018)
- Páginas: 485-487
- Seção: Crystal Growth
- URL: https://journals.rcsi.science/1063-7745/article/view/192596
- DOI: https://doi.org/10.1134/S106377451803029X
- ID: 192596
Citar
Resumo
The electrical conductivity of crystals of artificial cancrinite Na8 − 2xCax[Al6Si6O24][CO3] · 2H2O (x ≤ 0.03) has been studied in the temperature range of 498−604 K. These crystals were grown by hydrothermal synthesis on a seed in the Na2O–Al2O3–SiO2–H2O system (t = 380−420°С, P = 3 × 107−9 × 107 Pa). The ionic conductivity of a single-crystal sample (sp. gr. P63), measured along the crystallographic axis c, is low: σ = 8 × 10–7 S/cm at 300°С. The electric transport activation energy is Ea = 0.81 ± 0.05 eV. The relationship between the ionic conductivity and specific features of the atomic structure of cancrinites is discussed.
Sobre autores
N. Sorokin
Shubnikov Institute of Crystallography, Federal Scientific Research Centre “Crystallography and Photonics,”
Autor responsável pela correspondência
Email: nsorokin1@yandex.ru
Rússia, Moscow, 119333
Arquivos suplementares