Vickers microhardness of K2Co(SO4)2 · 6H2O single crystals and fracture geometry around impressions of vickers, knoop, and spherical indenters


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

The microhardness on the (010) and (001) planes in K2Co(SO4)2 · 6H2O crystal has been measured by the Vickers indentation method. Its values are, respectively, 11500 and 1300 MPa. No microhardness anisotropy of the first kind is revealed on either plane. The fracture geometry under indentation by a spherical indenter and Vickers and Knoop indenters is studied. The crystal has lower brittleness than the isomorphic Cs2Ni(SO4)2 · 6H2O crystal.

作者简介

N. Sizova

Shubnikov Institute of Crystallography

编辑信件的主要联系方式.
Email: nsizova37@mail.ru
俄罗斯联邦, Leninskii pr. 59, Moscow, 119933

N. Novikova

Shubnikov Institute of Crystallography

Email: nsizova37@mail.ru
俄罗斯联邦, Leninskii pr. 59, Moscow, 119933

V. Manomenova

Shubnikov Institute of Crystallography

Email: nsizova37@mail.ru
俄罗斯联邦, Leninskii pr. 59, Moscow, 119933

E. Rudneva

Shubnikov Institute of Crystallography

Email: nsizova37@mail.ru
俄罗斯联邦, Leninskii pr. 59, Moscow, 119933

A. Voloshin

Shubnikov Institute of Crystallography

Email: nsizova37@mail.ru
俄罗斯联邦, Leninskii pr. 59, Moscow, 119933

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Inc., 2016