Mechanical activation of crystallization of amorphous boron and synthesis of Al3Ti under cold isostatic pressing of B–Al–(LaB6–TiB2) powder
- Авторлар: Akimov G.Y.1, Soloviova T.A.2, Loboda P.I.2, Prilipko S.Y.1
-
Мекемелер:
- Galkin Donetsk Institute for Physics and Engineering
- National Technical University of Ukraine Igor Sikorsky Kiev Polytechnic Institute
- Шығарылым: Том 39, № 5 (2017)
- Беттер: 343-348
- Бөлім: Production, Structure, Properties
- URL: https://journals.rcsi.science/1063-4576/article/view/185975
- DOI: https://doi.org/10.3103/S1063457617050069
- ID: 185975
Дәйексөз келтіру
Аннотация
The powder mixture consisting of amorphous boron, crystalline aluminum, and a composite material LaB6–TiB2 is cold-isostatically-pressed under a pressure of up to 0.6 GPa and then heated to 1000°C. It is found out that almost the entire amount of amorphous boron contained in the mixture has been crystallized and the synthesis of Al3Ti has been noted, while the crystallization of amorphous boron usually occurs at a temperature of 1500°C.
Негізгі сөздер
Авторлар туралы
G. Akimov
Galkin Donetsk Institute for Physics and Engineering
Хат алмасуға жауапты Автор.
Email: tayzsolov@gmail.com
Украина, pr. Nauki 36, Donetsk, 03680
T. Soloviova
National Technical University of Ukraine Igor Sikorsky Kiev Polytechnic Institute
Email: tayzsolov@gmail.com
Украина, pr. Peremohy 37, Kiev, 03056
P. Loboda
National Technical University of Ukraine Igor Sikorsky Kiev Polytechnic Institute
Email: tayzsolov@gmail.com
Украина, pr. Peremohy 37, Kiev, 03056
S. Prilipko
Galkin Donetsk Institute for Physics and Engineering
Email: tayzsolov@gmail.com
Украина, pr. Nauki 36, Donetsk, 03680
Қосымша файлдар