Anodes for Lithium-Ion Batteries Obtained by Sintering Silicon Nanopowder
- Авторлар: Astrova E.V.1, Voronkov V.B.1, Rumyantsev A.M.1, Nashchekin A.V.1, Parfen’eva A.V.1, Lozhkina D.A.1
-
Мекемелер:
- Ioffe Institute
- Шығарылым: Том 55, № 3 (2019)
- Беттер: 184-193
- Бөлім: Article
- URL: https://journals.rcsi.science/1023-1935/article/view/191923
- DOI: https://doi.org/10.1134/S1023193519020010
- ID: 191923
Дәйексөз келтіру
Аннотация
Isochronous annealing of preliminarily compacted silicon nanopowder specimens is investigated. The density, structure, and conductivity of the material are determined as a function of sintering temperature. The electrochemical characteristics of anodes, which were sintered in the temperature range of 1100 to 1200°C, are studied using galvanostatic tests and cyclic voltammetry. It is found that the specimen, which was annealed at T = 1150°C, shows the best results. This specimen has a density of 1.60 g/cm3, a connected silicon framework, and an open-pore system.
Негізгі сөздер
Авторлар туралы
E. Astrova
Ioffe Institute
Хат алмасуға жауапты Автор.
Email: east@mail.ioffe.ru
Ресей, St. Petersburg, 194021
V. Voronkov
Ioffe Institute
Email: east@mail.ioffe.ru
Ресей, St. Petersburg, 194021
A. Rumyantsev
Ioffe Institute
Email: east@mail.ioffe.ru
Ресей, St. Petersburg, 194021
A. Nashchekin
Ioffe Institute
Email: east@mail.ioffe.ru
Ресей, St. Petersburg, 194021
A. Parfen’eva
Ioffe Institute
Email: east@mail.ioffe.ru
Ресей, St. Petersburg, 194021
D. Lozhkina
Ioffe Institute
Email: east@mail.ioffe.ru
Ресей, St. Petersburg, 194021
Қосымша файлдар