Investigations of the Defect Structures and g Factors for SnO2:Cr5+, SnO2:V4+, and TiO2:V4+ Crystals


Цитировать

Полный текст

Открытый доступ Открытый доступ
Доступ закрыт Доступ предоставлен
Доступ закрыт Только для подписчиков

Аннотация

The electron paramagnetic resonance (EPR) g factor formulas for SnO2:Cr5+, SnO2:V4+ and TiO2:V4+ crystals are deduced from Jahn–Teller effect and contributions of the charge-transfer levels. The tetragonal distortions ΔR = −0.0283, −0.0091, and −0.0045 nm, and Δθ = 0°, −0.0335°, and −0.0010°, for SnO2:Cr5+, SnO2:V4+ and TiO2:V4+, respectively. The calculations of the g factors agree well with the experimental values. The contributions of the charge-transfer levels to g factors increase with the increasing valence state. It must be taken into account in the precise calculations of g factors for the high-valence state d1 ions in crystals.

Об авторах

Lianxuan Zhu

School of Sciences, College of Sciences, Henan Agricultural University

Email: wmzk2002@163.com
Китай, NO. 95 Wenhua Road, Zhengzhou City, Henan Province, 450002

Minjie Wang

School of Sciences, College of Sciences, Henan Agricultural University

Автор, ответственный за переписку.
Email: wmzk2002@163.com
Китай, NO. 95 Wenhua Road, Zhengzhou City, Henan Province, 450002

Дополнительные файлы

Доп. файлы
Действие
1. JATS XML

© Springer-Verlag Wien, 2016

Согласие на обработку персональных данных

 

Используя сайт https://journals.rcsi.science, я (далее – «Пользователь» или «Субъект персональных данных») даю согласие на обработку персональных данных на этом сайте (текст Согласия) и на обработку персональных данных с помощью сервиса «Яндекс.Метрика» (текст Согласия).