Evaluation of the Fracture Toughness of Titanium Nitride Hardening Coatings According to Kinetic Indentation and Acoustic Emission Parameters


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

The possibility of the effective use of the kinetic indentation method in combination with the acoustic emission method for evaluating the fracture toughness of titanium nitride hardening coatings is shown. It is established that the occurrence of the first jog on the loading line of the kinetic indentation diagram in “load–indentor displacement–time” coordinates is due to the formation of the first crack in the coating and practically coincides in time with the occurrence of the acoustic emission impulse with an increased energy value. This permits a more accurate and substantiated determination of the critical load, indentation depth of the indentor, and hardness at which the first visible ring crack forms around the impression on the coating surface.

作者简介

V. Kachanov

National Research University – Moscow Power Engineering Institute (MPEI)

编辑信件的主要联系方式.
Email: KachanovVK@mail.ru
俄罗斯联邦, Moscow

I. Sokolov

National Research University – Moscow Power Engineering Institute (MPEI)

Email: KachanovVK@mail.ru
俄罗斯联邦, Moscow

V. Matyunin

National Research University – Moscow Power Engineering Institute (MPEI)

Email: KachanovVK@mail.ru
俄罗斯联邦, Moscow

V. Barat

National Research University – Moscow Power Engineering Institute (MPEI)

Email: KachanovVK@mail.ru
俄罗斯联邦, Moscow

V. Bardakov

National Research University – Moscow Power Engineering Institute (MPEI)

Email: KachanovVK@mail.ru
俄罗斯联邦, Moscow

A. Marchenkov

National Research University – Moscow Power Engineering Institute (MPEI)

Email: KachanovVK@mail.ru
俄罗斯联邦, Moscow

补充文件

附件文件
动作
1. JATS XML

版权所有 © Springer Science+Business Media, LLC, part of Springer Nature, 2017