Differential-Scanning Calorimetry of Anthracite, Graphite, and Calcium Salts
- 作者: Lopanov A.N.1, Kobzeva N.S.1, Fanina E.A.1, Nesterova N.V.1
-
隶属关系:
- Belgorod State Technological University
- 期: 卷 53, 编号 5 (2019)
- 页面: 308-313
- 栏目: Article
- URL: https://journals.rcsi.science/0361-5219/article/view/176965
- DOI: https://doi.org/10.3103/S0361521919050082
- ID: 176965
如何引用文章
详细
It was established that a shift of equilibrium in the graphite–calcium oxide system toward the formation of calcium carbide can be observed at a temperature of 900°C due to the formation of a volatile substance—carbon monoxide. Upon the addition of anthracite, a maximum of calcium carbonate decomposition decreased from 813 to 780°C, and the endothermic effect of the formation of calcium carbide manifested itself at 1350°C. In a mixture of calcium chloride with anthracite or graphite in stoichiometric amounts, the formation of calcium carbide and carbon tetrachloride was observed at 1100°C. The formation of calcium carbide was confirmed by chemical reactions of pyrolysis products with water (the release of acetylene) and by calculations of weight losses from thermogravimetric curves.
作者简介
A. Lopanov
Belgorod State Technological University
编辑信件的主要联系方式.
Email: alopanov@yandex.ru
俄罗斯联邦, Belgorod, 308012
N. Kobzeva
Belgorod State Technological University
编辑信件的主要联系方式.
Email: chemiezem@yandex.ru
俄罗斯联邦, Belgorod, 308012
E. Fanina
Belgorod State Technological University
编辑信件的主要联系方式.
Email: evgenia-@mail.ru
俄罗斯联邦, Belgorod, 308012
N. Nesterova
Belgorod State Technological University
Email: evgenia-@mail.ru
俄罗斯联邦, Belgorod, 308012
补充文件