The Distribution of Carbon in a Tungsten–Cobalt Alloy during Heat Treatment in a Gaseous Medium of Carbon Oxides


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

Investigations of composition, structure, and hardness of ultrafine-grained solid alloy WC–8Co–0.4VC–0.4Cr3C2 after treatment in a gaseous mixture of CO + CO2 of compacts with a lack of carbon for 50 min at a temperature 650°C on the initial stage of liquid-phase sintering. It was found that at CO content of 72.5% in the gas mixture, conditions are created for replacing the initial carbon deficiency (about 0.3%) and obtaining two-phase ultrafine-grained carbide of stoichiometric composition, in which carbon and hardness are uniformly distributed over the depth of the samples. This alloy has the lowest porosity (2.5%) and the highest hardness (HV1941). It was found that an increase of up to 80% or a decrease of up to 0% of the CO content in a gas mixture leads to the formation of a lack of carbon (1.0%) or an excess of carbon (4.5%) on the surface of the samples. This leads to a significant decrease in hardness. It is shown that the change in the carbon content and hardness in the depth of the samples is much less than on the surface.

Негізгі сөздер

Авторлар туралы

M. Dvornik

Institute of Materials Science, Khabarovsk Scientific Center, Far Eastern Branch, Russian Academy of Sciences

Email: alex-im@mail.ru
Ресей, Khabarovsk, 680042

A. Zaitsev

Institute of Materials Science, Khabarovsk Scientific Center, Far Eastern Branch, Russian Academy of Sciences

Хат алмасуға жауапты Автор.
Email: alex-im@mail.ru
Ресей, Khabarovsk, 680042

E. Mikhailenko

Institute of Materials Science, Khabarovsk Scientific Center, Far Eastern Branch, Russian Academy of Sciences

Email: alex-im@mail.ru
Ресей, Khabarovsk, 680042

Қосымша файлдар

Қосымша файлдар
Әрекет
1. JATS XML

© Pleiades Publishing, Ltd., 2019