Reduction of Silicon from a Ceramic Mold during Directional Solidification of Single-Crystal Nickel Superalloys
- 作者: Min P.1, Sidorov V.1, Vadeev V.1
-
隶属关系:
- All-Russia Institute of Aviation Materials (VIAM)
- 期: 卷 2018, 编号 13 (2018)
- 页面: 1288-1292
- 栏目: Processes of Manufacture of Ferrous and Nonferrous Metals
- URL: https://journals.rcsi.science/0036-0295/article/view/172840
- DOI: https://doi.org/10.1134/S0036029518130177
- ID: 172840
如何引用文章
详细
Silicon is one of the most harmful impurities in nickel superalloys used for casting aviation turbines: it decreases the high-temperature strength and the ductility. The reduction of silicon from a ceramic mold is experimentally studied during the directional solidification of a single-crystal nickel superalloy.
作者简介
P. Min
All-Russia Institute of Aviation Materials (VIAM)
编辑信件的主要联系方式.
Email: viamlab3@mail.ru
俄罗斯联邦, Moscow
V. Sidorov
All-Russia Institute of Aviation Materials (VIAM)
Email: viamlab3@mail.ru
俄罗斯联邦, Moscow
V. Vadeev
All-Russia Institute of Aviation Materials (VIAM)
Email: viamlab3@mail.ru
俄罗斯联邦, Moscow
![](/img/style/loading.gif)