Experiments on solid-phase pressure welding (PW) of a wrought EP975 nickel superalloy with a Ni3Al-based VKNA-25mono intermetallic alloy in a single-crystal state are performed under the superplasticity of the EP975 alloy, where its deformation was 24%. The structure and the phase composition of the interaction zone that forms between the materials to be joined after PW and PW followed by heat treatment are studied. The mechanical properties of the welded samples with a solid-phase joint are investigated. The ultimate tensile strength of the welded samples is shown to be 0.76 of the strength of the VKNA-25 alloy.

Об авторах

E. Galieva

Institute for Metals Superplasticity Problems, Russian Academy of Sciences

Автор, ответственный за переписку.
Email: galieva_elvina_v@mail.ru
Россия, Ufa, 450001

K. Povarova

Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences

Email: galieva_elvina_v@mail.ru
Россия, Moscow, 119334

A. Drozdov

Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences; Bardin Central Research Institute of Ferrous Metallurgy

Email: galieva_elvina_v@mail.ru
Россия, Moscow, 119334; Moscow, 105005

V. Valitov

Institute for Metals Superplasticity Problems, Russian Academy of Sciences

Email: galieva_elvina_v@mail.ru
Россия, Ufa, 450001


© Pleiades Publishing, Ltd., 2018

Данный сайт использует cookie-файлы

Продолжая использовать наш сайт, вы даете согласие на обработку файлов cookie, которые обеспечивают правильную работу сайта.

О куки-файлах