Interaction of exogenous refractory nanophases with antimony dissolved in liquid iron


Цитировать

Полный текст

Открытый доступ Открытый доступ
Доступ закрыт Доступ предоставлен
Доступ закрыт Только для подписчиков

Аннотация

The heterophase interaction of Al2O3 refractory nanoparticles with a surfactant impurity (antimony) in the Fe–Sb (0.095 wt %)–O (0.008 wt %) system is studied. It is shown that the introduction of 0.06–0.18 wt % Al2O3 nanoparticles (25–83 nm) into a melt during isothermal holding for up to 1200 s leads to a decrease in the antimony content: the maximum degree of antimony removal is 26 rel %. The sessile drop method is used to investigate the surface tension and the density of Fe, Fe–Sb, and Fe–Sb–Al2O3 melts. The polytherms of the surface tension of these melts have a linear character, the removal of antimony from the Fe–Sb–Al2O3 melts depends on the time of melting in a vacuum induction furnace, and the experimental results obtained reveal the kinetic laws of the structure formation in the surface layers of the melts. The determined melt densities demonstrate that the introduction of antimony into the Fe–O melt causes an increase in its compression by 47 rel %. The structure of the Fe–Sb–O melt after the introduction of Al2O3 nanoparticles depends on the time of melting in a vacuum induction furnace.

Об авторах

V. Burtsev

Baikov Institute of Metallurgy and Materials Science

Автор, ответственный за переписку.
Email: burtsev@ultra.imet.ac.ru
Россия, Leninskii pr. 49, Moscow, 119991

S. Anuchkin

Baikov Institute of Metallurgy and Materials Science

Email: burtsev@ultra.imet.ac.ru
Россия, Leninskii pr. 49, Moscow, 119991

A. Samokhin

Baikov Institute of Metallurgy and Materials Science

Email: burtsev@ultra.imet.ac.ru
Россия, Leninskii pr. 49, Moscow, 119991


© Pleiades Publishing, Ltd., 2017

Данный сайт использует cookie-файлы

Продолжая использовать наш сайт, вы даете согласие на обработку файлов cookie, которые обеспечивают правильную работу сайта.

О куки-файлах