Microstructure of a High-Strength Aluminum Alloy after Combined Surface Hardening


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

Carbide–boride coatings applied on both sides of V96Ts aluminum alloy samples by electric spark alloying (ESA) are metallographically studied. The coated samples are processed by laser on one side. Laser treatment of the surface decreases the pronounced roughness, pores, and cracks visible after ESA. Laboratory tests suggest combined (electric-spark–laser) hardening of the surface of V96Ts aluminum alloy samples to extend the service life of tools and machine parts.

Негізгі сөздер

Авторлар туралы

S. Kuptsov

Ural Federal University named after the first President B.N. Yeltsin

Email: neekeetina@mail.ru
Ресей, Yekaterinburg, 620002

A. Elantsev

Ural Federal University named after the first President B.N. Yeltsin

Email: neekeetina@mail.ru
Ресей, Yekaterinburg, 620002

E. Nikonenko

Ural Federal University named after the first President B.N. Yeltsin

Хат алмасуға жауапты Автор.
Email: eanik1311@mail.ru
Ресей, Yekaterinburg, 620002

E. Nikitina

Ural Federal University named after the first President B.N. Yeltsin; Institute of High-Temperature Electrochemistry, Ural Branch, Russian Academy of Sciences

Хат алмасуға жауапты Автор.
Email: neekeetina@mail.ru
Ресей, Yekaterinburg, 620002; Yekaterinburg, 620990

A. Shak

Ural Federal University named after the first President B.N. Yeltsin

Email: neekeetina@mail.ru
Ресей, Yekaterinburg, 620002

N. Kazakovtseva

Institute of High-Temperature Electrochemistry, Ural Branch, Russian Academy of Sciences

Email: neekeetina@mail.ru
Ресей, Yekaterinburg, 620990


© Pleiades Publishing, Ltd., 2019

Осы сайт cookie-файлдарды пайдаланады

Біздің сайтты пайдалануды жалғастыра отырып, сіз сайттың дұрыс жұмыс істеуін қамтамасыз ететін cookie файлдарын өңдеуге келісім бересіз.< / br>< / br>cookie файлдары туралы< / a>