Composition and structure of pyrophoric nickel catalysts according to X-ray diffraction data


Цитировать

Полный текст

Открытый доступ Открытый доступ
Доступ закрыт Доступ предоставлен
Доступ закрыт Только для подписчиков

Аннотация

The properties of a nickel catalyst obtained by treatment of nickel–aluminum alloy with sodium hydroxide in the presence of H2O2 and additionally stabilized with increased pressure were studied. Additional stabilization decreased the catalyst activity by 25%, but gave a more distinct picture for an XRD analysis of the active catalyst surface and decreased the time of deactivation of the dehydrated catalyst with air oxygen. The catalyst stabilization was explained by the displacement of water, decrease in the pore size, and surface inhomogeneity.

Об авторах

T. Osadchaya

Ivanovo State University of Chemical Technology

Email: afineevskiy@mail.ru
Россия, Ivanovo

A. Afineevskii

Ivanovo State University of Chemical Technology

Автор, ответственный за переписку.
Email: afineevskiy@mail.ru
Россия, Ivanovo

D. Prozorov

Ivanovo State University of Chemical Technology

Email: afineevskiy@mail.ru
Россия, Ivanovo

S. Kochetkov

Moscow State Technical University, Affiliation in Voskresensk

Email: afineevskiy@mail.ru
Россия, Moscow oblast

R. Rumyantsev

Ivanovo State University of Chemical Technology

Email: afineevskiy@mail.ru
Россия, Ivanovo

M. Lukin

Ivanovo State University of Chemical Technology

Email: afineevskiy@mail.ru
Россия, Ivanovo

Дополнительные файлы

Доп. файлы
Действие
1. JATS XML

© Pleiades Publishing, Ltd., 2017

Согласие на обработку персональных данных

 

Используя сайт https://journals.rcsi.science, я (далее – «Пользователь» или «Субъект персональных данных») даю согласие на обработку персональных данных на этом сайте (текст Согласия) и на обработку персональных данных с помощью сервиса «Яндекс.Метрика» (текст Согласия).