Formation of Compressed and Mixed-Layered Graphite on Heating Impact Diamonds


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

The graphitization process of impact diamonds in the helium atmosphere at 1900–1960 °C is investigated. It is shown that when an impact diamond particle with a large number of lonsdaleite defects is kept at 1900 °C for 1 min, ~5 wt.% of graphite are formed (in the paralle experiment with a particle without lonsdaleite defects the graphite formation is not observed). With an increase in the temperature to 1930 °С and 1940 °С the graphite amount increases to 70 wt.% and 80 wt.% respectively. In both cases, a mixture of two graphite phases forms: the first is turbostratic graphite with d002 = 3.38 Å; the second is compressed graphite with d002 = 3.21 Å. On heating a particle to 1960 °C graphite is formed in which the layer packing contains a large amount of defects and is a mixture of 2Н and 3R polytypes (the ratio 40:60) with a small degree of turbostratic disordering.

作者简介

S. Gromilov

Nikolaev Institute of Inorganic Chemistry, Siberian Branch; Novosibirsk State University

编辑信件的主要联系方式.
Email: grom@niic.nsc.ru
俄罗斯联邦, Novosibirsk; Novosibirsk

R. Nikolaev

Nikolaev Institute of Inorganic Chemistry, Siberian Branch

Email: grom@niic.nsc.ru
俄罗斯联邦, Novosibirsk

S. Cherepanova

Novosibirsk State University; Boreskov Institute of Catalysis, Siberian Branch

Email: grom@niic.nsc.ru
俄罗斯联邦, Novosibirsk; Novosibirsk

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2018