On the Mechanism of the Initial Stage of Titanium–Carbon Interaction


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

High-speed micro video recording and electron and atomic force microscopy have been used to obtain new experimental data at the initial stage of the titanium melt spreading along a carbon material (oriented pyrolytic graphite) and the formation of a reaction product. It has been shown that the melt spreading at the initial stages takes place along a framework of flat submicron crystalline grains of TiC with an open porosity. The grains form an island structure at the reagent contact boundary with gaps of about 100 nm in width between them, and these gaps are connected to each other to give a continuous network of channels along which the melt spreads. Thus, at the initial stage of the interaction, despite the formation of a solid product, direct contact of the reagents is retained, which ensures a high process speed.

作者简介

A. Rogachev

Merzhanov Institute of Structural Macrokinetics and Problems of Materials Science

编辑信件的主要联系方式.
Email: rogachev@ism.ac.ru
俄罗斯联邦, Chernogolovka, Moscow oblast, 142432

S. Vadchenko

Merzhanov Institute of Structural Macrokinetics and Problems of Materials Science

Email: rogachev@ism.ac.ru
俄罗斯联邦, Chernogolovka, Moscow oblast, 142432

N. Sachkova

Merzhanov Institute of Structural Macrokinetics and Problems of Materials Science

Email: rogachev@ism.ac.ru
俄罗斯联邦, Chernogolovka, Moscow oblast, 142432

E. Illarionova

Merzhanov Institute of Structural Macrokinetics and Problems of Materials Science

Email: rogachev@ism.ac.ru
俄罗斯联邦, Chernogolovka, Moscow oblast, 142432

V. Vagin

“Composite” Open Joint-Stock Company

Email: rogachev@ism.ac.ru
俄罗斯联邦, Korolev, Moscow oblast, 141070

V. Kostikov

Institute of Steel and Alloys “MISiS,”

Email: rogachev@ism.ac.ru
俄罗斯联邦, Moscow, 119049

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2018