A series of carbon-mineral composites with the carbon loading varying from 1.5 to 14.2 wt % has been synthesized by MgO carbonization in 1,3-butadiene at 600°C. The synthesized carbon-mineral composites have been studied by ESR, X-ray powder diffraction, and transmission electron microscopy. ESR has demonstrated that the MgO surface is completely covered with carbon after depositing 8–10 wt % C. MgO from the composite was dissolved by treatment with hydrochloric acid. The surface area of the carbon samples obtained after the acid treatment has been studied by thermal desorption of argon. It has been shown that the synthesized carbon material consists of a few graphene layers. The specific surface area of the synthesized graphene passes through a maximum of about 1800–1900 m2/g for samples obtained from C–MgO composites containing 8–10 wt % C.
作者简介
V. Chesnokov
Boreskov Institute of Catalysis, Siberian Branch,Russian Academy of Sciences
编辑信件的主要联系方式.
Email: chesn@catalysis.ru
俄罗斯联邦, Novosibirsk, 630090
A. Chichkan
Boreskov Institute of Catalysis, Siberian Branch,Russian Academy of Sciences
编辑信件的主要联系方式.
Email: AlexCsh@yandex.ru
俄罗斯联邦, Novosibirsk, 630090
A. Bedilo
Boreskov Institute of Catalysis, Siberian Branch,Russian Academy of Sciences
Email: AlexCsh@yandex.ru
俄罗斯联邦, Novosibirsk, 630090
E. Shuvarakova
Boreskov Institute of Catalysis, Siberian Branch,Russian Academy of Sciences
Email: AlexCsh@yandex.ru
俄罗斯联邦, Novosibirsk, 630090
V. Parmon
Boreskov Institute of Catalysis, Siberian Branch,Russian Academy of Sciences
Email: AlexCsh@yandex.ru
俄罗斯联邦, Novosibirsk, 630090
补充文件