Distribution of niobium and lanthanum between two immiscible melts in the system LaPO4–SiO2–NaF–Nb2O5–Fe2O3


如何引用文章

全文:

开放存取 开放存取
受限制的访问 ##reader.subscriptionAccessGranted##
受限制的访问 订阅存取

详细

The system LaPO4–SiO2–NaF–Nb2O5–Fe2O3 is characterized by immiscibility fields in the liquid state region. Addition of iron expands fields of immiscibility of melts and decreases the temperature of their coexistence. A fraction of 87–90% of niobium is extracted into iron silicate melt, and 92–98% of lanthanum is extracted into phosphate salt melt.

作者简介

L. Delitsyn

Joint Institute for High Temperatures

编辑信件的主要联系方式.
Email: delitzin@ihed.ras.ru
俄罗斯联邦, Moscow, 125412

补充文件

附件文件
动作
1. JATS XML

版权所有 © Pleiades Publishing, Ltd., 2017