Causes of Tube Heater (Finned Tube) Damage in the Production of Butyl Alcohol and Methanol Synthesis


Дәйексөз келтіру

Толық мәтін

Ашық рұқсат Ашық рұқсат
Рұқсат жабық Рұқсат берілді
Рұқсат жабық Тек жазылушылар үшін

Аннотация

Reasons are studied for breakdown and failure of tubular coil elements (finned tubes) designed for heating a production medium with flue gas heat before entering reaction columns. An analysis of cases of abnormal and emergency situations shows that cases of finned tube damage and breakdown occur predominantly due to infringement of operating regimes, changes in material properties during operation, and irregularities of the tube manufacturing process.

Авторлар туралы

A. Murashov

IrkutskNIIkhimmash Research Institute

Хат алмасуға жауапты Автор.
Email: al.o.murashov@gmail.com
Ресей, Irkutsk

A. Korchagin

IrkutskNIIkhimmash Research Institute

Email: al.o.murashov@gmail.com
Ресей, Irkutsk

N. Minenko

IrkutskNIIkhimmash Research Institute

Email: al.o.murashov@gmail.com
Ресей, Irkutsk

S. Demkin

IrkutskNIIkhimmash Research Institute

Email: al.o.murashov@gmail.com
Ресей, Irkutsk

A. Yudin

IrkutskNIIkhimmash Research Institute

Email: al.o.murashov@gmail.com
Ресей, Irkutsk


© Springer Science+Business Media New York, 2016

Осы сайт cookie-файлдарды пайдаланады

Біздің сайтты пайдалануды жалғастыра отырып, сіз сайттың дұрыс жұмыс істеуін қамтамасыз ететін cookie файлдарын өңдеуге келісім бересіз.< / br>< / br>cookie файлдары туралы< / a>